Carbide spade drill to drill out hardened steel
Only 4 geometries to grind on a broken carbide endmill shank and you can drill out hardened steel.
Inspired by Sandvik hardcut and OSG tap extracting drills
Syndicated from the fediverse. Read and engage on the original instance.
View original on lemmy.worldOnly 4 geometries to grind on a broken carbide endmill shank and you can drill out hardened steel.
Inspired by Sandvik hardcut and OSG tap extracting drills
1 reply
Neat guide, thanks for sharing!