top-layer delamination solved by lower speed

I had some severe delamination a.k.a layer separation but specifically on the top layer

The slicer's profile for my printer set top-level speed to 200 mm/s so I halved it, and now there's almost no delamination at all

View original on lemmy.ml
10

1 reply

Lower speed means less flow through the nozzle and warmer plastic. It will have more time at the melting temperature and therefore stick better to the previous layer.